Abstract

Low-modulus β-type Ti‑Nb alloys reduce the elastic modulus mismatch with bone, but their bioinert surface must be functionalized, and the role of the pulse duty cycle in micro‑arc oxidation (MAO) of calcium phosphate coatings on such alloys remains unclear. In this work, the pulse on-time was varied from 80 to 1600 μs at a fixed voltage of 300 V, frequency of 125 Hz, and treatment time of 10 min, which raised the duty cycle from 1 to 20 % and the cumulative energized time from 6 to 120 s. Coatings were deposited on ultrafine‑grained Ti‑45Nb from an acidic electrolyte containing dispersed Ca9Zn1(PO4)6(OH)2 (Zn‑HA) particles. A 20‑fold increase in energized time produced only a 5-fold increase in thickness, from 45 ± 3.2 to 225 ± 5.0 μm. The coatings consist of hollow spheroids that grow with the duty cycle and contain monetite (CaHPO4) as the only crystalline calcium phosphate detected, consistent with the Ca / P ratio of 0.91 measured inside fractured spheroids. The scratch critical load increased 8-fold, to 63 N, and the corrosion current density in 0.9 % NaCl at 37°C decreased 8-fold, to (3.90 ± 0.65) ·10−8 A / cm2. The polarization resistance reached a maximum of 1.07 ·106 Ω·cm2 at 15 % duty cycle and did not improve further at 20 %, where the lower corrosion current was offset by a smaller Stern–Geary coefficient. Thickness therefore ceases to control the barrier performance above approximately 200 μm. Duty cycles of 10 –15 % give the best balance among the measured structural, mechanical, and electrochemical properties, whereas the porous layers grown at higher duty cycles may potentially be better suited as anchoring or reservoir layers rather than as diffusion barriers.
Funding
1. Program for the development of the world‑class scientific center “New Materials for Special Purposes” - subsidy agreement No. 075‑15‑2025‑589