Effect of forging routes and heat treatment on the microstructure and mechanical properties of an advanced β-solidifying γ-TiAl alloy

Получена 23 октября 2026; Принята 03 ноября 2026;
Эта работа написана на английском языке
Цитирование: D.M. Trofimov, V.M. Imayev, R.M. Imayev. Effect of forging routes and heat treatment on the microstructure and mechanical properties of an advanced β-solidifying γ-TiAl alloy. Письма о материалах. 2026. Т.16. №4. С.462-469
BibTex   https://doi.org/10.48612/letters/2026-4-462-469

Аннотация

Tensile properties of the alloy in microstructural conditions obtained via different forging routes followed by an identical heat treatment as a function of the test temperature: (a) elongation, (b) ultimate tensile strength (UTS)The effect of forging and heat treatment on the microstructure and mechanical properties of an advanced β-solidifying γ-TiAl alloy with a nominal composition of Ti-44.5Al-7(Nb, Zr, Ta, Hf)-0.1B (at.%) was investigated. The initial material was produced as small laboratory as-cast ingots. The ingots were subjected to isothermal single- or multistage 3D forging at 950°C, followed by an identical heat treatment. Processing resulted in the formation of coarser and finer-grained duplex microstructures that were nearly free of the β / β0 phase. Microstructural analysis suggested the following solidification and solid-state phase transformation pathway: L → L+β → β → β+α → α+βm → α+γ+βm → α+γ+β0m → α2+γ+β0m, where βm / β0m represents the retained metastable β / β0 phase. Mechanical testing demonstrated that multistage 3D forging followed by heat treatment yielded superior tensile properties compared to its single-stage counterpart. In particular, the room-temperature ultimate tensile strength (UTS) and ductility (El) after 3D forging and heat treatment reached 804 MPa and 1.85 %, respectively, compared to 745 MPa and 1.0 % for the condition obtained via single-stage forging. Concurrently, the creep tests at 750 and 800°C showed higher creep resistance of the alloy in state obtained via single-stage forging, which is attributed to coarser microstructure and a higher lamellar constituent. The enhanced tensile performance of the finer-grained material is attributed to a more delocalized character of plastic deformation, which suppresses premature failure. At elevated temperatures (750 – 800°C), however, the higher density of grain / colony boundaries in the finer microstructure obtained via 3D forging likely facilitated grain / colony boundary sliding, thereby shifting the brittle-to-ductile transition towards low temperatures and reducing creep resistance.

Ссылки (26)

17. Metallography of Titanium Alloys (ed. by N. F. Anoshkin), Moscow, Metallurgy, 1980, 464 p. (in Russian) [Н. Ф. Аношкин, Металлография титановых сплавов, Москва, Металлургия, 1980, 464 c.].
18. F. Appel, J. D. H. Paul, M. Oehring, Gamma Titanium Aluminide Alloys: Science and Technology, Wiley-VCH, Weinheim, 2011, 745 p.

Финансирование на английском языке